Stabilizing Catalytic Pt-OH-Fe(III) Interfaces by Mesoporous TiO2 with Rich Surface Hydroxyl Groups
Wu Qingyuana, Qin Ruixuana, Zang Dandana, Zhang Wuyonga, Wu Binghuib, Zheng Nanfenga
a Department of Chemistry, College of Chemistry and Chemical Engineering, Xiamen University, Xiamen 361005, China;
b Pen-Tung Sah Institute of Micro-Nano Science and Technology, Xiamen University, Xiamen 361005, China
Received 2018-04-16  Revised null