Acta Chimica Sinica Previous Articles     Next Articles

高性能生物基聚酯弹性体的软段设计与性能研究

王梦月a, 唐银繁a, 杨琴a, 陈胜a, 房玉庆*,b, 阎斌*,a   

  1. a四川大学 轻工科学与工程学院,四川 成都 610065;
    b健帆生物科技集团股份有限公司,广东 珠海 519085
  • 投稿日期:2026-07-08

Soft Segment Design and Performance of High-Performance Bio-Based Polyester Elastomers

Mengyue Wanga, Yinfan Tanga, Qin Yanga, Sheng Chena, Yuqing Fang*,b, Bin Yan*,a   

  1. aCollege of Light Industry Science and Engineering, Sichuan University, Chengdu, Sichuan 610065;
    bJianfan Biotechnology Group Co., Ltd., Zhuhai, Guangdong 519085
  • Received:2026-07-08
  • Contact: *E-mail: fangyuqing@jafron.com; yanbinscu@126.com

The high strength and high elastic recovery of thermoplastic polyester elastomers (TPEEs) are often difficult to achieve simultaneously. To address this challenge, a series of bio-based polyester elastomers were designed and synthesized via Knoevenagel polycondensation at a relatively low temperature of 190 °C. Three model soft segments with distinctly different chain structures, including polycaprolactone diol (PCL, crystallizable polyester type), polytetrahydrofuran (PTMG, amorphous polyether type), and polycarbonate diol (PCDL, amorphous polycarbonate type), were derivatized into monomers with identical cyano end groups and subsequently copolymerized with a bio-based rigid dialdehyde hard segment derived from vanillin. The chemical structures of the monomers and resulting elastomers were confirmed by nuclear magnetic resonance (NMR) spectroscopy and Fourier transform infrared (FTIR) spectroscopy. The thermal properties were characterized by thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC). The microphase separation behavior was investigated by dynamic mechanical analysis (DMA), wide-angle X-ray diffraction (WAXD), and atomic force microscopy (AFM). The mechanical properties were evaluated by uniaxial tensile tests, and the solvent resistance was assessed by immersion tests in solvents with different polarities. Among the three elastomers, the PCDL-based elastomer exhibited outstanding mechanical performance, achieving a tensile strength of 24.2 MPa and an elongation at break of 663%. WAXD, DMA, and AFM characterizations consistently confirmed the formation of well-ordered structures within the PCDL-based system, which constructed a robust and tough network responsible for the excellent mechanical properties. In contrast, the PCL-based elastomer showed a tensile strength of 21.8 MPa and an elongation at break of 830%, while the PTMG-based elastomer exhibited a tensile strength of 18.8 MPa and an elongation at break of 1200%. The PCDL-based elastomer also demonstrated the highest glass transition temperature (-8 °C) and the widest rubber plateau in DMA, indicating the most thermally stable physical crosslinking network. This study offers a new approach to overcoming the strength-elasticity trade-off in bio-based elastomers through rational soft segment design.

Key words: Thermoplastic polyester elastomer, Knoevenagel polycondensation, Polycarbonate diol, High strength, High elastic recovery