share
Acta Chimica Sinica ›› 1982, Vol. 40 ›› Issue (3): 233-242. Previous Articles Next Articles
徐晓白, 彭美生, 曹嘉正
投稿日期:
发布日期:
通讯作者:
XU XIAO-BAI(H. P. HSU), PENG MEI-SHENG, GAO JIA-ZHENG
Received:
Published:
Share
The reactions of LaB6 and CeB6 with CO2 at the temperature range of 500-1000℃ have been studied by means of thermogravimetry, chemioal analysis and X-ray analysis, eto. It has been found that these hexaborides are stable under CO2 below 700℃ and reaotion manifests itself above 700℃. With the mentioned temperature range, the main reaction may be expressed by equation(1).
XU XIAO-BAI(H. P. HSU), PENG MEI-SHENG, GAO JIA-ZHENG. THE REACTION OF LANTHANUM HEXABORIDE AND CERIUM HEXABORIDE WITH CARBON DIOXIDE AT HIGH TEMPERATURE[J]. Acta Chimica Sinica, 1982, 40(3): 233-242.