化学学报 ›› 2009, Vol. 67 ›› Issue (17): 1957-1961. 上一篇    下一篇

研究论文

三维有序大孔α-Fe2O3的制备及电化学性能研究

赵铁鹏 高德淑* 雷钢铁 李朝晖

  

  1. (湘潭大学化学学院 环境友好化学与应用省部共建教育部重点实验室 湘潭 411105)

  • 投稿日期:2009-02-07 修回日期:2009-03-21 发布日期:2009-09-14
  • 通讯作者: 高德淑

Fabrication and Electrochemical Properties of Three-dimensionally Ordered Macroporous α-Fe2O3

Zhao, Tiepeng Gao, Deshu* Lei, Gangtie Li, Zhaohui   

  1. (Key Laboratory of Environmentally Friendly Chemistry and Applications of Ministry of Education, College of Chemistry, Xiangtan University, Xiangtan 411105)

  • Received:2009-02-07 Revised:2009-03-21 Published:2009-09-14
  • Contact: Gao, Deshu

通过聚苯乙烯(PS)胶晶模板法合成了三维有序大孔(3DOM) α-Fe2O3, 运用扫描电镜、热重分析、X射线衍射、电化学充放电等多种方法对其结构和性能进行了表征和研究. SEM表明PS 胶晶模板和3DOM α-Fe2O3呈周期性排列. 合成的3DOM α-Fe2O3为三维有序多孔网状结构, 具有球型和六边形的孔隙形貌, 其孔径大小约为(115±10) nm; 孔壁由α-Fe2O3纳米晶粒组成, 壁厚为20~30 nm. XRD图谱表明经过煅烧除去模板后, 形成了纯α-Fe2O3相. 当3DOM α-Fe2O3作为锂离子电池负极材料时, 首次放电充电容量分别高达1880和1130 mAh•g-1, 20次循环后可逆容量依然高达631 mAh•g-1, 库仑效率大于90%.

关键词: 模板, 大孔, α-Fe2O3, 锂离子电池, 负极材料

Three-dimensionally ordered macroporous (3DOM) α-Fe2O3 was synthesized by using polystyrene (PS) colloidal crystal as templates. The character of 3DOM α-Fe2O3 was measured by scanning electron microscopy (SEM), thermogravimetry (TG), X-ray diffraction (XRD) and electrochemical measurements. SEM images showed that the PS colloidal crystal template and the 3DOM α-Fe2O3 were arrayed periodically in face. The synthesized 3DOM α-Fe2O3 microparticles were composed of sphere or hexagonally porous morphologies interconnected through thin walls formed by nanocrystals of α-Fe2O3. The macropore diameters of the 3DOM α-Fe2O3 were about (115±10) nm and the pore wall thicknesses were between 20~30 nm. X-ray diffraction indicated that a pure α-Fe2O3 phase was produced after calcination. When the 3DOM α-Fe2O3 microparticles were used as anode materials for lithium ion batteries, they exhibited extraordinarily high initial discharge and charge capacities of 1880 and 1130 mAh•g-1 respectively. After 20th cycle, their reversible capacity could be as high as 631 mAh•g-1, with a coulombic efficiency of >90%.

Key words: template, macroporous, α-Fe2O3, lithium ion battery, anode material