Sonochemical Gold Coating of Fe3O4 Nanoparticles and Its Characterizations

WU Wei1; HE Quan-Guo*,1; CHEN Hong1,2; TANG Jian-Xin1; NIE Li-Bo1   

  1. (1 Green Packaging and Biological Nanotechnology Laboratory, Hunan University of Technol-ogy, Zhuzhou 412008)
    (2 College of Life Science and Technology, Central South University of Forestry & Technology, Changsha 410004)
  • Received:2006-11-21 Revised:2007-01-23 Published:2007-07-14
  • Contact: HE Quan-Guo

Air-stable nanoparticles Fe3O4/Au have been prepared via sonolysis of a solution of hydrogen tetrachloroaureate(III) trihydrate (HAuCl4) and (3-aminopropyl)triethoxysilane (APTES)-coated Fe3O4 nanoparticles with further drop-addition of sodium citrate. The Fe3O4/Au nanoparticles have been characterized by X-ray powder diffraction (XRD), ultraviolet-visible spectroscopy (UV-Vis), scanning elec-tron microscopy (SEM) with the energy dispersive spectroscopy (EDS), transmission electron microscopy (TEM), X-ray photoelectron spectroscopy (XPS) and superconducting quantum interference device (SQUID) magnetometry. Fe3O4/Au nanoparticles obtained under appropriate conditions possess a very high saturation magnetization of about 63 emu•g-1, and their average diameter was about 30 nm.

Key words: Fe3O4/Au magnetic nanoparticle, gold coating, sonochemical synthesis, surface modification, magnetic property, magnetite